| Glass type | ECR | ||||||
| Sizing type | Silane | ||||||
| Typical filament diameter(㎛) | 13 | 14 | 16 | 17 | |||
| Typical linear density(tex) | 200/300 | 230 | 600/1200 | 800 | |||
| Example | ECDR13-300-810 | ||||||
| Item | Linear density variation | Moisture content | Combustible content | Breakage strength |
| Unit | ㎛ | % | % | (N/Tex) |
| Test method | ISO 1889 | ISO 3344 | ISO 1887 | ISO 3341 |
| Standard range | ±4 | ≤0.10 | 0.40~0.70 | ≥0.4 |










| Glass type | ECR | ||||||
| Sizing type | Silane | ||||||
| Typical filament diameter(㎛) | 13 | 14 | 16 | 17 | |||
| Typical linear density(tex) | 200/300 | 230 | 600/1200 | 800 | |||
| Example | ECDR13-300-816H | ||||||
| project | linear density deviation | Moisture content | Combustible content | stiffness |
| unit | ㎛ | % | % | (mm) |
| Detection method | ISO 1889 | ISO 3344 | ISO 1887 | ISO 3341 |
| index | ± 4 | ≤0.10 | 0.40~0.70 | ≥0.45 |










| Glass type | ECR |
| Sizing type | Silane |
| Typical filament diameter(㎛) | 13 |
| Typical linear density(tex) | 2400 |
| Example | ECR13-2400-911 |
| project | linear density deviation | Moisture content | Combustible content | stiffness |
| unit | ㎛ | % | % | (mm) |
| Detection method | ISO 1889 | ISO 3344 | ISO 1887 | ISO 3341 |
| index | ±5 | ≤0.10 | 0.35~0.65 | 120±20 |